Pengaruh waktu tahan pada proses tempering terhadap kekuatan impak baja s45c


Oleh : Fadli Abdat

Info Katalog

Penerbit : FTI - Usakti

Kota Terbit : Jakarta

Tahun Terbit : 2019

Pembimbing 1 : Dody Prayitno

Subyek : Mechanical engineering;Metals;Tempering

Kata Kunci : impact test, tempering, oil, quenching, holding time

Status Posting : Published

Status : Lengkap


File Repositori
No. Nama File Hal. Link
1. 2019_TA_STM_061001400087_Halaman-Judul.pdf
2. 2019_TA_STM_061001400087_Lembar-Pengesahan.pdf
3. 2019_TA_STM_061001400087_Bab-1_Pendahuluan.pdf 4
4. 2019_TA_STM_061001400087_Bab-2_Tinjauan-Pustaka.pdf
5. 2019_TA_STM_061001400087_Bab-3_Metodologi-Penelitian.pdf
6. 2019_TA_STM_061001400087_Bab-4_Analisis-Hasil-dan-Pembahasan.pdf
7. 2019_TA_STM_061001400087_Bab-5_Kesimpulan-dan-Saran.pdf
8. 2019_TA_STM_061001400087_Daftar-Pustaka.pdf
9. 2019_TA_STM_061001400087_Lampiran.pdf

B Baja JIS S45C (JIS : Japanese Industrial Standard) merupakan jenis baja “Medium CarbonSteel” banyak digunakan karena harganya yang lebih murah dari machinery steel lainnya.Untuk mendapatkan sifat yang diinginkan, logam terlebih dahulu diberikan perlakuan panassesuai dengan kebutuhan. Tujuan dari penelitian ini untuk mengetahui nilai kekuatan tarikdan kekerasan serta struktur mikro. Baja S45C yang telah diuji komposisi kimianya diberiperlakuan panas hardening pada temperature 900°C. Kemudian di quenching menggunakanmedia oli. Masing-masing benda uji yang telah mengalami proses pendinginan tersebut,kemudian diberi perlakuan tempering hingga 400°C dengan holding time 1 jam dan 2 jam.Selanjutnya dilakukan uji impak dengan metode charpy dan dilakukan pengujian metalografiuntuk mengetahui strukturmikro dari baja S45C. Dari hasil penelitian didapatkan nilaiketangguhan yang paling besar adalah 47.56 Joule didapatkan dari material yang diberikanperlakuan tempering 2 jam. Nilai kekerasan yang paling besar adalah 302.1 HV didapatkandari material yang diberikan perlakuan tempering 1 jam. Raw material memiliki nilaiketangguhan dan kekerasan yang paling rendah. Pemberian perlakuan tempering berpengaruhterhadap kekerasan dan ketangguhan.

J JIS Steel S45C (JIS: Japanese Industrial Standard) is a type of "Medium Carbon Steel" whichis widely used because the price is cheaper than other machinery steels. To obtain the desiredproperties, the metal is first given heat treatment according to the needs. The purpose of thisstudy is to determine the value of tensile strenght and hardness, also microstructure. S45Csteel that has been tested for its chemical composition is given a hardening heat treatment at900°C. The next step is quenching treatment using oil media. Each specimen that hasexperienced a cooling process, is then given a tempering up to 400°C with a holding time of1 hour and 2 hours. Then the impact test is conducted using the charpy method andmetallographic testing is carried out to determine the microstructure of S45C steel. Theresults of this study show that the biggest value of toughness is 47.56 Joules obtained fromthe material given a two hour tempering treatment. The biggest hardness value is 302.1 HVobtained from materials that are given one hour tempering treatment. Raw material has thelowest value of toughness and hardness. Thus, tempering treatment affects hardness andtoughness.