Analisis perubahan karakteristik ring washer alumunium pada baut pengurasan oli untuk penggunaan beruang
R Ring washer aluminium digunakan sebagai pencegahan kebocoran pada baut penutup lubang pengurasan oli mesin atau oli transmisi kendaraan bermotor. setelah baut dikencangkan, ring washer terdeformasi plastis menutup celah antara kepala baut dengan ulir lubang baut pada wadah oli (oil pan). Ring washer semestinya hanya digunakan sekali pakai dan diganti baru apabila dilakukan pengurasan oli. Penelitian tentang perubahan karakteristik ring washer, sebelum digunakan, setelah diberikan beban 67,8 Nm, setelah dilakukan pembebanan torsi dua kali masing - masing 67,8 Nm dengan proses annealing dan diberikan pembebanan torsi dua kali masing - masing 67,8 Nm. Dari hasil penelitian didapat bahwa ring washer dapat digunakan berulang apabila dilakukan proses annealing, untuk menurunkan nilai kekerasannya, apabila tidak dilakukan proses annealing maka secara fisik dan nilai kerasnya berubah menjadi 240% dari sampel as it is. Deformasi yang terjadi sebesar 25,56% dari sampel as it is. Deformasi yang terjadi sebesar 24,56% dari sampel as it is menjadi sampel dengan pembebanan torsi dua kali masing – masing 67,8 Nm.
A Aluminum washer rings are used to prevent leakage in the bolts to cover the engine oil drain holes or motor vehicle transmission oil. After the bolt is tightened, the washer is plastically deformed to close the gap between the bolt head and the screw hole thread in the oil pan. The ring washer should only be used once and replaced with a new one when draining the oil. Research on changes in the characteristics of the ring washer, before being used, after being given a load of 67.8 Nm, after being subjected to torsion loading twice with 67.8 Nm each with the annealing process and being given a torsion load twice each of 67.8 Nm. From the results of the study, it was found that the ring washer can be used repeatedly if the annealing process is carried out, to reduce the hardness value, if the annealing process is not carried out, the physical and hardness value changes to 240% of the as it is sample. The deformation that occurs is 25.56% of the sample as it is. The deformation that occurs is 24.56% of the as-it-is sample into a sample with a torsion loading twice of 67.8 Nm each.