DETAIL KOLEKSI

Studi pengaruh variasi pH pada proses flotasi bijih galena

3.0


Oleh : Taufan Anggara

Info Katalog

Nomor Panggil : 738/TT/2020

Penerbit : FTKE - Usakti

Kota Terbit : Jakarta

Tahun Terbit : 2020

Pembimbing 1 : Subandriao

Pembimbing 2 : Christin Palit

Subyek : Galena;Ore deposits

Kata Kunci : galena, flotation, XRF (X-Ray Fluorence), pH (Power of Hydrogen), recovery,

Status Posting : Published

Status : Lengkap


File Repositori
No. Nama File Hal. Link
1. 2020_TA_STT_073001900086_Halaman-Judul.pdf 17
2. 2020_TA_STT_073001900086_-Pengesahan.pdf
3. 2020_TA_STT_073001900086_Bab-1_Pendahuluan.pdf 5
4. 2020_TA_STT_073001900086_Bab-2_Tinjauan-Literatur.pdf
5. 2020_TA_STT_073001900086_Bab-3_Karangka-Konsep.pdf
6. 2020_TA_STT_073001900086_Bab-4_Metode.pdf
7. 2020_TA_STT_073001900086_Bab-5_Kesimpulan.pdf
8. 2020_TA_STT_073001900086_Daftar-pustaka.pdf 1
9. 2020_TA_STT_073001900086_Lampiran.pdf

P Proses konsentrasi berdasarkan secara flotasi dapat meningkatkan kadar bijih galena yang memiliki kandungan galena rendah yaitu 2-8%. Denganpenelitian ini menggunakan bijih galena dari Purwakarta Jawa Barat dapatmeningkatkan kandungan galena. Hasil penelitian ini menggunakan alat flotasidengan proses mengapungan atau dikeluarkan sebagai konsentrat dari mineralberharga dengan kondisi flotasi yang tetap yaitu : sampel, pH, kecepatan putar1500 rpm, frother pine oil 1 tetes, collector Dicresyl(D25) 0,07 gram, Depressant0,23 gram, dan 0,30 gram, waktu flotasi 8 menit. Sedangkankondisi flotasi dibuat bervariasi pH yaitu: pH 6, pH 7, pH 8, pH 9, pH 10. Hasilflotasi atau feed ataupun konsentrat menggunakan X-ray Flourosence (XRF) danX-ray Diffraction (XRD) untuk memperoleh kadar unsur dan senyawa yang ada.Didapat kadar timbal pada variasi pH dan feed adalah feed (10,54%), 200 meshpH 6 (22,08%), 200 mesh pH 7 (26,23%), 200 mesh pH 8 (27,22%), 200 mesh pH9 (30,16%), 200 mesh pH 10 (23,34%). Hasil dari perhitungan recoverymetallurgical balance dari berbagai pH nilai terbaik adalah di pH 7 (32,27%).

T The process of concentration based on flotation can increase the levels ofgalena ore which has a low galena content of 2-8%. With this research usinggalena ore from Purwakarta, West Java, can increase the content of galena. Theresults of this study use a flotation device with a floating process or released as aconcentrate of valuable minerals with fixed flotation conditions: sample, pH, 1500rpm rotational speed, frother pine oil one drop, collector Dicresyl (D25) 0.07gram, Depressant 4 0,23 gram and 0,30 gram, flotation time 8minutes. While the flotation conditions are varied, they are: pH 6, pH 7, pH 8, pH9, pH 10. The results of the flotation or feed or concentrate use X-rayFluorescence (XRF) and X-ray Diffraction (XRD) to obtain elemental content andexisting compounds. Lead content obtained at variations in pH and feed is feed(10.54%), 200 mesh pH 6 (22.08%), 200 mesh pH 7 (26.23%), 200 mesh pH 8(27.22%), 200 mesh pH 9 (30.16%), 200 mesh pH 10 (23.34%). The results of thecalculation of metallurgical balance recovery from various pH values are best atpH 7 (32.27%).

Bagaimana Anda menilai Koleksi ini ?